I <br /> 28-Day Compressive Maximum 200 psi. <br /> Strength <br /> Unit Mass (Wet) 80 to 110 pcf I <br /> Temperature, Minimum at 50 degrees F (10 degrees C) <br /> Point of Delivery <br /> C. Provide water content in design mix to produce self-leveling, flowable fill material at time of <br /> placement. <br /> D. Design mix air entrainment and unit mass are for laboratory design mix and source quality <br /> control only. <br /> 2.5 SOURCE QUALITY CONTROL I <br /> A. Test and analyze properties of flowable fill design mix and certify results for the following: <br /> 1. Design mix proportions by weight of each material. <br /> 2. Aggregate: ASTM C33 for material properties and gradation. I <br /> 3. Properties of plastic flowable fill design mix including: <br /> a. Temperature. ' <br /> b. Slump. <br /> c. Air entrainment. <br /> d. Wet unit mass. <br /> e. Yield. <br /> f. Cement factor. <br /> 4. Properties of hardened flowable fill design mix including: <br /> a. Compressive strength at 1 day, 7 days, and 28 days. Report compressive strength of <br /> each specimen and average specimen compressive strength. <br /> b. Unit mass for each specimen and average specimen unit mass at time of compressive <br /> strength testing. <br /> B. Prepare delivery tickets containing the following information: <br /> 1. Project designation. <br /> 2. Date. <br /> 3. Time. <br /> 4. Class and quantity of flowable fill. <br /> 5. Actual batch proportions. <br /> 6. Free moisture content of aggregate. <br /> 7. Quantity of water withheld. <br /> I <br /> i <br /> Legion Golf Course Stormwater Detention Project Flowable Fill <br /> WO#UP3620 31 23 24-4 <br />